Low sintering godhong PTFE unmelted, nyebabake mikro-pori, adhesion miskin, lumahing atos, kekuatan mechanical kurang, lan katon milky. Overheating ngrusak PTFE, ngasilake pinholes, umpluk, brittleness, werna kuning-ireng, lan asap beracun. Loro-lorone ngrusak kompak, kinerja non-stick, keluwesan, insulasi, lan stabilitas dimensi. Kisaran optimal 370–400°C ngasilake lapisan semi-transparan, mulus, tan. Priksa visual: matte putih = under-sintered; kuning / brittle = over-sintered. (296 aksara)