Raws li cov kws tshaj lij kev tsim khoom ntawm PTFE kub kub ntaub, Jiangsu Aokai Cov Khoom Tshiab qhia txog kev paub txog kev lag luam nrog koj. Ntug warping thiab ntog tawm ntawm PTFE high kub tapes yog tsis tshua muaj tshwm sim los ntawm ib qho tseem ceeb, tab sis tshwm sim los ntawm kev sib xyaw ua ke ntawm kev xaiv daim kab xev tsis zoo, kev sib raug zoo ntawm qhov chaw tsis zoo, txoj kev ua haujlwm tsis raug thiab kev pabcuam hnyav. Hauv qab no yog cov laj thawj tsis ua haujlwm thiab cov kev daws teeb meem sib xws:
Feem ntau ua tsis tiav ntawm PTFE High Temperature Daim kab xev |
Targeted Solutions |
Cov nplaum nplaum tsis raug xaiv: Acrylic-raws li PTFE daim kab xev siv nyob rau hauv kev ua haujlwm kub kub |
Xaiv silicone nplaum nplaum PTFE daim kab xev rau ib puag ncig saum 120 ℃; acrylic nplaum hom tsuas yog siv tau rau kev siv qhov kub thiab txias |
Inferior nplaum zoo nrog tsawg viscosity thiab tsis zoo thermal stability |
Ua qhov ntsuas kub kub ua haujlwm ua ntej yuav khoom; xaiv cov khoom los ntawm cov tuam txhab muaj npe nrov thiab txheeb xyuas lawv cov kev ua haujlwm kub adhesion |
Cov kab mob sib kis tau npog nrog cov roj stains, plua plav, dej cim los yog cov kua nplaum qub qub |
Ua tib zoo ntxuav qhov chaw nrog isopropyl cawv los yog anhydrous ethanol thiab tag nrho nws qhuav ua ntej pasting; ib qho dej noo yuav ua rau cov nyhuv sib khi tsis muaj zog |
Mismatched nto roughness tsis ua tiav cov nplaum nplaum txaus |
Polish overly du nto kom zoo; qib ntxhib nto los yog txais yuav 0.18-0.25mm tuab PTFE daim kab xev los sau qhov khoob |
Cov txheej txheem pasting tsis raug: ntau dhau ntawm zaj duab xis nruj, tsis txaus nias thiab tso pa tawm, kev tsim kho kub qis lossis rov ua dua. |
Siv qhov nro nruab nrab thaum lub sij hawm lamination, dov khov kho nrog cov menyuam siab kom tshem tawm cov npuas npuas; preheat qhov chaw rau 20-25 ℃ ua ntej pasting nyob rau hauv qis kub; zam tev thiab rov ua daim kab xev |
Qhov kub thiab txias ntau dhau: kev pabcuam ntev tshaj 260 ℃ lossis kub kub hloov pauv |
Tswj kev khiav hauj lwm kub tsis tu ncua nyob rau hauv 260 ℃, lub sij hawm luv luv ncov kub tsis tshaj 300 ℃ thiab kav ntev dua 1 feeb; txais yuav ua tau zoo silicone nplaum daim kab xev ntxiv rau txhua yam fixation rau loj kub txawv scenarios |
Nyuaj heev thiab tuab substrate tsis tuaj yeem haum rau qhov nkhaus lossis qhov tsis sib xws |
Ua ntej nyias-hom PTFE daim kab xev ntawm 0.08-0.13mm rau cov xwm txheej uas yuav tsum tau muaj kev sib haum xeeb |
Kev khaws cia tsis raug ua rau cov nplaum nplaum ua rau ntxov ntxov nyob rau hauv qhov kub thiab txias, av noo thiab ncaj qha tshav ntuj |
Khaws cov ntaub nplaum kaw rau hauv qhov chaw txias thiab qhuav ntawm qhov kub zoo ntawm -5 ~ 38 ℃ thiab av noo ntawm 30% ~ 70% RH |
Rau daim kab xev nrog me ntsis ntug warping, koj tuaj yeem nias lub warped qhov chaw hauv zos nrog cov menyuam, los yog siv cov cua kub me me hauv qab 60 ℃ los txhim kho adhesion rau kev siv thaum muaj xwm ceev. Thaum cov nplaum txheej deteriorates, hloov thiab rov pasting yog tsim nyog.
Roj stains thiab plua plav yuav cais cov nplaum txheej ntawm lub hauv paus nto. So saum npoo nrog high-purity hnyav thiab ua kom tiav ziab. Nruab nrab roughening ntawm du cov menyuam nto tuaj yeem txhim kho adhesion.
Cua cov kab xev nrog nruj nruj; Kev nruj nruj heev yuav ua rau tsis tu ncua shrinkage thiab ntug lifting.Roll tusyees ntawm ib kawg mus rau lwm yam tam sim ntawd tom qab haum kom tshem tawm tag nrho cov huab cua npuas thiab xyuas kom meej tag nrho wetting ntawm nplaum thiab substrate.Finish pasting nyob rau hauv ib tug mus. Re-sticking yuav txo tau qhov qub kev sib raug zoo zog.
Khaws qhov ntsuas kub ntawm qhov ntsuas kub ntawm 20-30 ℃ txawm rau qib siab PTFE tapes. Lub sij hawm ntev overheating yuav ua rau cov tshuaj degradation thiab embrittlement ntawm silicone nplaum, uas yog lub ntsiab ua rau tsis ua hauj lwm mus tas li. Siv cov clamps thiab lwm txoj hauv kev kho kom haum raws li qhov kub thiab txias hloov. Tsis tas li ntawd, paub meej tias cov tshuaj tiv thaiv ntawm daim kab xev thaum siv nyob rau hauv ib puag ncig uas muaj zog alkali, ketone los yog ester cov kuab tshuaj; silicone nplaum backed tapes khav theeb zoo dua compatibility.
Nyob rau hauv luv luv, daws ntug lifting thiab tev cov teeb meem nyob rau hauv lub hauv paus ntawm kev xaiv cov khoom raug, tsim qauv thiab nruj kev ua hauj lwm mob tswj. Xaiv cov nplaum nplaum uas haum raws li qhov kev pab cuam qhov kub thiab txias yog qhov tseem ceeb lav rau daim ntawv thov ruaj khov ntawm PTFE high temperature tapes.
Kab lus no yog muab los ntawm Jiangsu Aokai Tshiab Materials Technology Co., Ltd.
Yog tias koj xav tau cov ncauj lus kom ntxaws, daim ntawv thov cov lus qhia thiab cov kev daws teeb meem rau peb cov khoom lag luam suav nrog PTFE kub ntaub, PTFE kub daim kab xev, PTFE kub mesh siv, seamless fusing tshuab siv, ib sab PTFE daim ntaub, kub resistant conveyor siv thiab kub resistant fiberglass daim ntaub, thov hu rau peb:
· Mr. Guo: +86 18944819998
· Mr. Liu: +86 13705266308
Peb ib txwm txhawb nqa qhov kev pabcuam kev tshaj lij ntawm kev tshaj lij thiab kev ncaj ncees, thiab muab koj nrog ib qho kev lag luam daws teeb meem thiab kev xav txog kev pabcuam tag nrho.