2026-05-28 PTFE surface treatment for bonding adhesion uses two main methods: high-temperature melting (superior weather resistance, 9.5 MPa strength with coupling agent, but releases toxic gases) and sodium-naphthalene etching (5 MPa immediate adhesion, narrow 24-48 hour window, hazardous waste). Choose based on environmental control and long-term vs. short-term performance.
Read More
2026-05-27 Testing PTFE emulsion quality involves six key indicators: solid content (60±2% per T/FSI 067-2021), pH (9.0-11.0), particle size distribution (laser diffraction/DLS), viscosity (12-30 mPa·s at 25°C), stability (centrifugal, thermal, freeze-thaw), and appearance. This guide covers standard test methods for each parameter.