Ile » Iroyin » PTFE alemora teepu Silikoni PSA Lẹhin Arugbo-Iwọn otutu: Agbara Peeli ati Iṣọkan nipasẹ Ipele

Silikoni PSA Lẹhin Arugbo-Iwọn otutu: Agbara Peeli ati Iṣọkan nipasẹ Ipele

Awọn iwo: 0     Onkọwe: Aago Atẹjade Olootu Aaye: 2026-06-08 Oti: Aaye

Beere

Nigbati a Teepu alemora iwọn otutu ti PTFE ni a lo ni agbegbe ti o gbona - sọ, 200 ° C fun awọn ọsẹ tabi awọn oṣu - alemora titẹ-sensitive silikoni (PSA) le yipada. Agbara Peeli le dide, ṣubu, tabi gbigbe iyokù. Iṣọkan le pọ si (brittleness) tabi dinku (ikuna iṣọpọ).

Kii ṣe gbogbo awọn PSA silikoni huwa kanna. Awọn iyato wa si isalẹ lati polima tiwqn (methyl vs. methylphenyl), crosslinking siseto (peroxide vs. afikun arowoto), ati awọn ipin ti MQ resini to roba.

Aokai PTFE nlo ọpọ awọn ipele PSA silikoni ninu awọn teepu wa. Itọsọna yii ṣe alaye ohun ti o ṣẹlẹ si peeli agbara ati isọdọkan lẹhin ti ogbo otutu otutu fun ipele kọọkan, ati bii o ṣe le yan eyi ti o tọ fun ohun elo rẹ.

Silikoni_PSA_Tape_High_Temp_Aging.png

Kini o ṣẹlẹ si Silikoni PSA Labẹ Ooru - Awọn ipo Ikuna Meji

Nigbati o ba dagba ni iwọn otutu giga (200-250°C), awọn PSA silikoni le ṣe awọn ayipada idakeji meji:

1. Lilọ kiri-lẹhin (dari si brittleness)

Awọn ẹgbẹ iṣẹ ṣiṣe ti ko dahun tẹsiwaju lati fesi, jijẹ iwuwo crosslink. Agbara peeli ibẹrẹ le dide fun igba diẹ, lẹhinna ṣubu ni mimu bi alemora ṣe di lile. Agbara rirẹ-ara aimi han lati pọ si, ṣugbọn didimu agbara ati resistance resistance bajẹ. Fiimu alemora di lile ati dojuijako.

2. Ibajẹ eegun ẹhin (o yori si ipadanu peeli ati iyokù)

Egungun ẹhin polydimethylsiloxane gba cyclization ati scission pq. Agbara Peeli ṣubu nigbagbogbo. Alemora le gbe lọ si sobusitireti ( iyoku) tabi kuna ni iṣọkan. Eyi jẹ wọpọ ni awọn PSA silikoni methyl-kekere.

Awọn paramita iṣatunṣe bọtini:

  • Akoonu Phenyl (ti o ga ju = resistance ooru to dara julọ)

  • Ìwúwo Crosslink ati iru imularada (afikun imularada vs. peroxide ni arowoto)

  • Ipin ti resini MQ si rọba silikoni

Ipe Classifications nipa Kemikali Be

1. Standard polydimethylsiloxane (methyl-Iru silikoni PSA)

  • Idaduro Peeli lẹhin ti ogbo (200-250 ° C): Agbara Peeli ga soke die-die ni akọkọ, lẹhinna kọ. Lẹhin awọn ọjọ 7 ni 250 ° C, idaduro peeli jẹ 50-70% nikan . Iṣe n lọ silẹ ni iyara ni awọn iwọn otutu ti o ga julọ. Ibajẹ wa lati cyclization ti ẹhin dimethyl siloxane.

  • Iduroṣinṣin isomọ: Awọn ẹya ti a mu-iwosan-peroxide (fun apẹẹrẹ, KR-101) ni awọn olupilẹṣẹ ti o ku ti o fa imudanu lẹhin-itọju – alemora lile ati embrittles. Agbara rirẹ akọkọ ni ilọsiwaju, ṣugbọn didimu agbara silẹ, ati ikuna iṣọpọ waye labẹ ooru. Awọn ẹya ti a ṣe arowoto ni diẹ dara ṣugbọn ṣi ni opin nipasẹ ailagbara igbona atorunwa ti ẹhin dimethyl.

2. Methylphenyl polysiloxane (iwọn sooro iwọn otutu giga)

  • Idaduro Peeli lẹhin ti ogbo: Awọn ẹwọn ẹgbẹ Phenyl ṣe idilọwọ iṣakojọpọ deede ti awọn apakan dimethyl ati dinku ibajẹ cyclization. Lẹhin awọn ọjọ 7 ni 250°C, idaduro agbara peeli kọja 85% . Awọn agbekalẹ giga-phenyl ṣetọju awọn ohun-ini peeli iduroṣinṣin paapaa ni 260-288 ° C.

  • Iduroṣinṣin iṣọkan: O tayọ. Agbara rirẹ yipada ni iwonba; dani idaduro agbara koja 80%. Layer alemora si maa wa rọ gun-igba lai embrittlement tabi aloku. Awọn giredi giga-phenyl ti a ṣe iwosan ni afikun jẹ PSA silikoni iduroṣinṣin Ere.

Methyl_vs_Methylphenyl_Silicone_Aging_Chart.png

3. Peeli-giga pataki ati awọn ipele aṣa-kekere

  • Awọn ipele peeli giga (fun apẹẹrẹ, Dow 7385, peeli aṣoju> 10N / 25mm): Ikojọpọ resini MQ ti o ga julọ funni ni tack ibẹrẹ ti o dara julọ ati peeli agbara, ṣugbọn ni idiyele ti resistance ooru ati iduroṣinṣin isomọ. Wọn ṣe afihan peeli ti o tobi ju lẹhin ti ogbo ati pe o ni itara si iyokù nitori jijẹ gbigbona resini. Lo nikan fun awọn ohun elo kekere-iwọn igba diẹ.

  • Peeli-kekere, awọn ipele fiimu aabo isomọ giga: iwuwo crosslink giga n funni ni iṣẹ peeli iduroṣinṣin ati iduroṣinṣin ti ogbo ti o dara julọ, ṣugbọn taki ibẹrẹ kekere. Lẹhin ti ogbo, wọn wa ni iṣọkan ṣugbọn di lile, dinku ibamu si awọn aaye ti o ni inira.

High_Peel_Silicone_PSA_Residue_Transfer.png

Isẹ-ọna Ikọja – Peroxide vs. Iwosan Itọju Afikun (Ipilẹ Methyl Kanna)

Paapaa pẹlu polima methyl kanna, ọna imularada ni iyalẹnu yipada ihuwasi ti ogbo.

1. Peroxide-iwosan (iran ibẹrẹ ti aṣa)

  • Peroxide ti o ku nfa isakoṣo lẹhin-crosslinking lakoko ti ogbo iwọn otutu.

  • Peeli agbara spikes lakoko, lẹhinna ṣubu ni mimu.

  • Isomọ dide ni igba diẹ, atẹle nipa embrittlement ati didimu ikuna agbara.

  • Aitasera ti ogbo ipele-si-ipele ko dara.

2. Imudara-afikun (hydrosilylation curing)

  • Ni arowoto gbogbo ko si byproducts; crosslink nẹtiwọki jẹ gbọgán Iṣakoso.

  • Awọn iyipada ohun-ini lẹhin-ti ogbo tẹle aṣa laini asọtẹlẹ kan.

  • Idaduro peeli ti o ga julọ ati iduroṣinṣin isomọ ni akawe si awọn agbekalẹ peroxide.

Peel_Strength_Aging_Curve.png

Ite Yiyan Itọsọna

Ipò Iṣẹ

Niyanju ite

Kí nìdí

Tẹsiwaju iwọn otutu giga (> 200°C), peeli iduroṣinṣin, iyoku odo

Itọju-pada sipo, phenyl giga (fun apẹẹrẹ, Dow 7388, Q2-7406)

> 85% peeli idaduro, ko si embrittlement,> 80% idaduro agbara

Ooru giga igba diẹ igba diẹ, iye owo-kókó

Iru methyl boṣewa, afikun-iwosan, imularada lẹhin-lẹhin (fun apẹẹrẹ, 7657)

Iṣe itẹwọgba ṣugbọn nireti diẹ ninu ibajẹ peeli ati embrittlement ti o ṣeeṣe lori awọn iyipo gigun

Peeli ibẹrẹ ti o ga pupọ nilo, iwọn otutu kekere nikan

Giga-peeli methyl ite

Ko fun lemọlemọfún ga ooru; reti aloku lẹhin ti ogbo

Fiimu aabo, isọpọ giga, tack kekere

Giga-crosslink kekere-peeli ite

Iduroṣinṣin ti ogbo ti o dara ṣugbọn lile ati pe ko ni ibamu

Iṣeduro Aokai PTFE : Fun eyikeyi teepu PTFE ti yoo rii awọn iwọn otutu ti o duro loke 200°C, pato afikun-iwosan methylphenyl silikoni PSA. Iye owo iwaju ti ga julọ, ṣugbọn o ṣe idiwọ awọn ikuna aaye ti o ṣẹlẹ nipasẹ iyoku alemora tabi pipadanu mnu.

Lakotan – Imudara Silikoni PSA ite si Ibeere Gbona

  • PSA silikoni iru-ara Methyl (paapaa peroxide-ni arowoto) dara nikan fun igba diẹ tabi lilo iwọn otutu kekere. Lẹhin awọn ọjọ 7 ni 250 ° C, reti pipadanu 30-50% peeli ati didasilẹ ti o ṣeeṣe.

  • Methylphenyl (high-phenyl) silikoni PSA da duro> 85% agbara peeli ati isomọ rọ lẹhin ti ogbo kanna. O jẹ yiyan fun iṣẹ lilọsiwaju 200-250 ° C.

  • Ilana ọna asopọ agbelebu ṣe pataki pupọ: imularada afikun (hydrosilylation) jẹ iduroṣinṣin diẹ sii ju imularada peroxide lọ.

  • Awọn ipele peeli-giga ṣe iṣowo pipa iduroṣinṣin ti ogbo fun taki akọkọ - yago fun wọn ni awọn ohun elo gbona.

Fun wiwa isọdọkan iwọn otutu giga, Aokai PTFE nlo awọn PSAs silikoni methylphenyl ti a mu-iwosan ni afikun. A le pese data idaduro peeli lẹhin 1000h ni 250 ° C lori ibeere.

Imọ akoonu pese nipa Jiangsu Aokai New Materials Technology Co., Ltd.

Fun alaye alaye awọn iwe data imọ-ẹrọ ati awọn solusan aṣa fun awọn aṣọ iwọn otutu giga PTFE, awọn teepu, awọn beliti mesh, ati diẹ sii:

Ni ibamu si iṣẹ-ṣiṣe ati iduroṣinṣin, a pese awọn solusan adani-iduro kan ati awọn iṣẹ lẹhin-tita ni ironu.

Ọja iṣeduro

Ọja Ìbéèrè

Awọn ọja ti o jọmọ

Jiangsu Aokai Ohun elo Tuntun
AoKai PTFE jẹ alamọdaju PTFE Ti a bo Fiberglass Fabric Awọn iṣelọpọ ati awọn olupese ni Ilu China, amọja ni ipese PTFE alemora teepu, PTFE Conveyor igbanu, PTFE Mesh igbanu . Lati ra tabi osunwon PTFE ti a bo fiberglass fabric awọn ọja. Ọpọlọpọ iwọn, sisanra, awọn awọ wa ti adani.

Awọn ọna asopọ kiakia

Ẹka Ọja

PE WA
Adirẹsi: Zhenxing  Road, Dasheng Industrial Park, Taixing 225400, Jiangsu, China
 Tẹli:  +86 18796787600
Imeeli  :  vivian@akptfe.com
Tẹli: +86 13661523628
Imeeli   mandy@akptfe.com
Oju opo wẹẹbu: www.aokai-ptfe.com
Aṣẹ-lori-ara ©   2024 Jiangsu Aokai New Materials Technology Co., Ltd. Gbogbo ẹtọ wa ni ipamọ Maapu aaye