Kahor dahaarka PTFE, impregnation resin, ama lamination, marada fiberglass-ka ah waa in horay loo qalajiyey. Ujeeddadu waxa ay noqon kartaa in si fudud qoyaanka looga saaro, ama waxa ku lug lahaan kara gubidda walxaha cabbirka dharka (dewaxing), ama in dharka lagu diiriyo heerkul deggan ka hor inta aan la damin. Ujeedo kastaa waxay u baahan tahay heerkul kala duwan iyo habayn waqti.
Xuduudaha aan saxda ahayn waxay u horseedi karaan dhalmo la'aan, isku xirnaanta daciifka ah, huruuda dharka, luminta xoogga - ama xitaa xoqin dhamaystiran.
Aokai PTFE waxay leedahay waayo-aragnimo balaadhan oo ku saabsan farsamaynta fiber galaaska. Hagahan waxa uu sharxayaa saddexda qaybood ee daawaynta ugu waaweyn, heerkulkooda ugu fiican, xakamaynta wakhtiga, iyo talooyinka la taaban karo ee natiijooyinka joogtada ah.
Ujeedada daawaynta |
Kala duwanaanta heerkulka |
Ujeedada Muhiimka ah |
Codsiyada caadiga ah |
|---|---|---|---|
Ka saarista qoyaanka (inta badan) |
105°C – 120°C |
Ka saar biyaha la isku daray adiga oo aan waxyeello u geysan walxaha cabbirka |
Lamination, daahan PTFE/silicone, diyaarinta diyaarinta |
Nadiifinta wax-ka-saarista / kulaylka (saarista cabbirka) |
300°C – 450°C |
Si buuxda u gubi cabbirka dharka (starch, PVA, iwm.) |
Nidaamyada u baahan dusha sare ee nadiifka ah: impregnation resin, daaweynta kiimikada |
Kuleylinta ka hor wareejinta habka |
60°C – 100°C |
Kor u qaad heerkulka dharka si loogu dahaadho ama uumi u yeesho |
Khadadka dahaarka joogtada ah, ka hor taangiyada ku shubista xabagta; waxay ka hortagtaa viscosity resin ka kaca marada qabow |
Tani waa tillaabada qallajinta ee caadiga ah ee inta badan dharka ka hor dahaarka ama dahaadhka. Hadafku waa qoyaan si fiican loo nadiifiyo iyadoo la ilaalinayo walxaha cabbirka ee isku haya fiilooyinka.
Dharka elektiroonigga ah ee guud iyo xoojinta: ilaali 105°C – 120°C.
Dharka lagu daweeyay walxaha isku xidha silane : heerkulka ka dhig 110°C si aad isaga ilaaliso in aad jebiso xidhmooyinka isku xidhka.
Wejiga heerkulka foornada dhexdeeda waa in lagu xakameeyaa ±5°C gudahood si looga hortago kulaylka deegaanka.
Miisaanka Dharka |
Waqtiga lagu taliyay |
|---|---|
Dhar khafiif ah (<100 g/m²) |
10 - 15 daqiiqo |
Dhexdhexaad & dhar culus (200 - 400 g/m²) |
20 - 30 daqiiqo |
Dhar qaro weyn / dermo (> 600 g/m²) |
1-2 saacadood ama ka badan |
Heerka joojinta: Miisaanka joogtada ah waxaa la gaaraa marka farqiga miisaanka u dhexeeya laba cabbir oo isku xigta uu ka yar yahay 0.1%. Dharka duuban, si dabacsan u daldali ama isticmaal xariijimaha meelaha bannaan inta lagu jiro qalajinta si aad uga fogaato dhibaatada dibadda engegan laakiin gudaha qoyan.
Foornada waa in ay qasab ku demisaa . Fur hawo-mareenada hawada cusub si ay hawada qoyan ugu soo daayaan waqtigii loogu talagalay.
Ha xad-dhaafin foornada; Hubi socodka hawada wareeg kasta ama warqad kasta.
Marka maradu ay tahay in ay gebi ahaanba xor ka ahaato walxaha cabbirka organic (tusaale, ka hor inta aan la saarin resin impregnation ee hawada hawada ama isku-darka heerkulka sare), nadiifinta kulaylka ayaa loo baahan yahay.
Kacsanaanta & heerka sigaarka: qiyaastii 300°C. Waxay u baahan tahay ogsijiin ku filan iyo qiiq waxtar leh.
Marxaladda gubashada harta: si tartiib tartiib ah kor ugu qaad heerkulka ilaa 380 ° C - 450 ° C oo qabo, si buuxda u oksijiye kaarboonka haraaga ah.
Weligaa ha dhaafin 500°C – haddii kale muraayadda lafteedu waxay noqonaysaa mid jajaban oo dhaawacmi doonta.
Foornooyinka kululaynta ee joogtada ah, hagaaji xawaaraha socodka dharka si aad u hubiso in maradu ku sii jirto aagga heerkulka sare dhowr ilaa toban daqiiqo, taas oo ku xidhan miisaanka dharka. Dharka culculus waxay u baahan yihiin soo-gaadhsiin dheer.
Khasaaraha shilka (LOI) waa in ka yar 0.1%. Tani waa heerka dahabka.
Tijaabada goobta fudud: Ku shidi gees dhar ah oo iftiin leh. Walxaha u qalma ma soo saaraan qiiq madow ama ur gaar ah, oo leh hadhaaga dambaska ugu yar.
Dharka u qalma wuxuu u muuqdaa caddaan ama wuxuu hayaa midabkiisii asalka ahaa, iyada oo aan lahayn dhibco madow ama jaalle ah.
Dharka muraayadda laga demay waxay leedahay hawl sare oo dusha sare ah . Isla markiiba u wareeji habka soo-jiidashada, ama si fiican u xir oo xir si aad uga hortagto dib u nuugista qoyaanka iyo wasakheynta.
Kahor intaadan codsan emulsion PTFE ama daahan silikoon ah, dharku wuxuu u baahan karaa kulayl tartiib ah heerkul deggan.
Deji heerkulka: 60°C – 80°C , waxyar ka sarraysa barta sayaxa ambient si aad uga fogaato qalajinta dusha sare ee dahaarka.
Waqtiga deganaanshaha: badiyaa daraasiin ilbiriqsi ilaa hal ama laba daqiiqo iyada oo loo sii marayo foornooyinka infrared-gaaban ama hawo kulul - kaliya waxay ku filan tahay inay dharka u keento heerkulka bartilmaameedka.
U qaado heerkulka dharka dhabta ah sida heerka caadiga ah, ee ha u qaadan heerkulka hawada foornada. Isticmaal heerkulbeegyada infrared ama aaladaha cabbiraadda heerkulka la socodka wakhtiga dhabta ah.
Socodka hawada isku midka ah & wareegga wareegga - hawo kululaynta ayaa go'aamisa waxtarka qallajinta. Xawaaraha dabaysha ee lebbiska ahi waxa ay hubisaa in xataa heerkulku kala qaybiyo ballaca dharka.
Tijaabada muunada hordhaca ah: Dufcooyin kala duwan ayaa laga yaabaa inay isticmaalaan walxaha cabbirka kala duwan. Qaado muunado yaryar oo ku qalaji heerkul kala duwan (105°C, 120°C, 130°C, iwm.). U fiirso midabka dusha sare iyo isbeddelka xoogga si aad u xaqiijiso heerkulka ugu sarreeya ee dufcad kasta.
Dharka la qalajiyey, gaar ahaan maro la demay, ayaa nadiif ah oo si fudud u wasakhaysan.
Haddi aan si degdeg ah loo isticmaalin, bacaha aluminiumka ku xidh qallajiyaha.
Beddelka: ku kaydi qolka qalajinta oo heerkulkiisu ka hooseeyo 30°C iyo huurka qoyaanka ah ee ka hooseeya 40%.
Daaqada isticmaalka lagu taliyay: 4 ilaa 8 saacadood gudahood ka dib qalajinta natiijooyinka ugu fiican. Wixii intaas ka dambeeya, dib u qalaji ka hor intaanad isticmaalin.
Tilmaanta Aokai PTFE: Codsiyada la isku halleyn karo ee sarreeya (isku-dhafka hawada sare, dahaarka korantada sare), waxaan kugula talineynaa inaad isticmaasho dharka isla markiiba ka dib qalajinta ama 2 saacadood gudahood.
Habka |
Heerkulka |
Waqtiga (miisaan ahaan) |
Jeegaga Muhiimka ah |
|---|---|---|---|
Ka saarida qoyaanka |
105-120°C (<110°C ee silane-daaweeyay) |
10-30 daqiiqo (dhuuban ilaa dhexdhexaad); 1-2 saac (culus) |
Miisaanka joogtada ah (<0.1% isbeddel); qoyaanka qasabka ah |
Nadiifinta wax-ka-qabashada / kulaylka |
300-450C (waligeed>500°C) |
Dhowr ilaa 10+ daqiiqo |
LOI <0.1%; ma jiro qiiq madow; caddaan/muuqaal nadiif ah |
Kuleylinta ka hor dahaarka |
60-100°C |
Ilbiriqsi ilaa 2 daqiiqo |
heerkulka maro la qiyaasay; socodka hawada isku midka ah |
Kaydinta qallajinta ka dib |
<30°C, <40% RH |
Isticmaal 4-8 saacadood gudahood |
Bacaha xiran ama qolka qalajinta |
Aokai PTFE waxay siisaa qeexitaan qallajin ka hor dhammaan maro-gilaasyadayada. Codsiyada muhiimka ah, waxaan ku siin karnaa dhar hore loo qallajiyey oo faakuum-shaaban oo diyaar u ah isticmaalka degdega ah. Nala soo xiriir si aad u hesho cabbirada qalajinta caadada ah ee ku saleysan nooca dharkaaga iyo habka xiga.
Nuxurka kore waxaa bixiya Jiangsu Aokai New Materials Technology Co., Ltd.
Haddii aad rabto inaad wax badan ka ogaato faahfaahinta faahfaahsan, xaaladaha codsiga iyo xalalka loo habeeyey ee noocyada kala duwan ee alaabtayada, oo ay ku jiraan PTFE dhar heerkul sare ah, cajalado heerkul sare ah PTFE, suumanka mesh PTFE, suumanka mashiinka isku-xidhka ah, maro PTFE hal dhinac ah, heerkul sare oo u adkaysta gudbinta iyo suumanka fiberglaska ah fadlan nala soo xiriir.
Mudane Guo: +86 18944819998
Mudane Liu: +86 13705266308
Waxaan had iyo jeer taageernaa falsafada xirfad-yaqaannimada iyo daacadnimada, waxaana naga go'an inaan ku siino xal hal-joojin ah iyo adeegyo feker leh.