Ukubuka: 0 Umbhali: Isikhathi Sokushicilela Isihleli Sesayithi: 2026-07-14 Umsuka: Isayithi
Okuqukethwe
1.Inhloso: Ukuqeda ngokuphelele ukususwa kwezinto eziphilayo njenge-paraffinwaxandoilskusuka phezulu kwefayibha, ngaleyo ndlela kwephule umgoqo phakathi kokulapha kanye nefayibha yengilazi.
2.Indlela: I-fiberglass yafihlwa ngokuqhubekayo noma ama-batchesinanovenge ku-300°C–450°C. Uma izinga lokushisa liphansi, liyancibilika lizobe lingaphelele; uma izinga lokushisa liphakeme kakhulu noma ubude besikhathi liphansi kakhulu, intambo izolimala kakhulu.
3.Imibandela yokwahlulela ye-PTFE abakhiqizi bendwangu enezinga lokushisa eliphezulu: Indwangu elashiwe kufanele ibonakale emhlophe noma i-lightlytan. Kukhona futhi izingxenye ezimbili ezidingekayo ngokwesilinganiso ukuze zibe ngaphansi kuka-0.2%, zikhiqiza lokho okwaziwa ngokuthi'indwangu ekhishwa ngewax eshisayo' noma'.
1.Corestep: I-Couplingagenttreatment.Imvamisa kusetshenziswa ama-silanecouplingagents(isb,KH-550,KH-560,A-174,njll.)aphinde asetshenziswe.I-heat-dewaxedfiberglassfabricisimmersedinalow- ukugxilisana okunamanzi okuhlanganisa isixazululo, kulandelwangokomisa ukuvumela ukuhlanganisanakugoqe futhi kuphulukiswe ebusweni befayibha, kwakha ifilimu yekhemikhali.
2.Qaphela: Indwangu yengilazi yengilazi ethengiswayo eminingi enezinsimbi eziqinisiwe(isb, izindwangu ezilukiwe zisuka ekuqondiseni)sezivele zinakho lokhu kwelashwa sekuqediwe efektri,okungakhishwa ngayo.Nokho,lokhu kufanele kuqinisekiswe.
1.Ukomisa/Ukususa umswakama: I-fiberglass fabricishighlyhygroscopic.Ngaphambi kokumithiswa,kumele ilale ku-80°C–120°C amahora angu-1–2ukugcina umswakama wokuqukethwe ube ngaphansi kuka-0.1%.Indwangu elashiwe kufanele ibe sebenzisa ngokushesha noma igcine idiza isitaki ukuze ivimbele ukumunca futhi ukumunca umswakamo.
2.Ukushisa ngaphambili: Akudingekile, kodwa kuvame ukusetshenziswa ekucubunguleni i-spultrusion, filamentwinding, kanye ne-RTM(resintransfermolding).Inhloso yokuvimbela ukubukeka kwe-viscosity kungazelelwe kukhuphule okunye okunye othintana naye ngendwangu ebandayo, engase ikhinyabeze ukuphuma okumanzi.Izinga lokushisa elingaphambi kokushisa 6°C-40°
1.Ukusika: Sika ngokuhambisana nesandla esidizayinelwe ubukhulu-ama-angles, futhi uqinisekise ukuthi uqaqa izintambo noma umshini obukhali uyasuswa ngokuhlanzekile.
2.Ukuhlanza: Khipha ama-chips nothuli olukhiqizwe ngesikhathi sokusika.Ngezinhlelo zokusebenza ezidingeka kakhulu ezifana nokufakwa kukagesi noma imikhiqizo esobala, ubuso kufanele busulwe ngendwangu yamahhala noma ehlanzekile enomoya ocindezelwe.
3.Ukuqedwa kokuqina: Imvelo, i-fiberglassfabrictendstogeneratestaticelectricityekhanga uthuli.Iyanconywa ukusebenzisaimishini yokuqeda i-static efana nezinsimbi zomoya.
Ulwazi olungenhla luhlinzekwa nguI-JiangsuAokaiNewMaterialTechnologyCo.,Ltd.
Uma ungathanda ukuthola-ulwazi olujulile lwemikhiqizo egcwele-okuhlanganisa indwangu ye-Teflonhigh-temperature,Teflonhigh-temperaturetape,Teflonhigh-temperaturemeshbelt,amabhande angenamthungo emishini yokubopha,indwangu yohlangothi olulodwaPTFE, amabhande okuthutha amelana namazinga okushisa aphezulu, indwangu yengilazi yengilazi ekwazi ukumelana nezinga lokushisa eliphezulu, nokunye–kanye nemininingwane ecacisiwe, izimo zohlelo lokusebenza, nezisombululo zokwenza ngendlela oyifisayo, sicela uzizwe ukhululekile ukuthintana ngalezi ziteshi ezilandelayo: